Title: Thermoelectric Application of Temperatures on Models of Concrete Structures

Author(s): Gilbert L. Butler

Publication: Special Publication

Volume: 25

Issue:

Appears on pages(s): 301-307

Keywords: concretes; loads (forces); microconcrete; models; mortars (material); temperature; thermal gradient; thermal stresses; thermoelectricity; research

Date: 1/1/1971

Abstract:
Research into methods by which temperature changes could be applied to structural models of concrete structures led to the use of a commerically manufactured solid state heat pump commonly known as a thermoelectric module.