The Modulus of Concrete and the Coefficient of Expansion of Concrete and Reinforced Concrete at Below Normal Temperatures

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: The Modulus of Concrete and the Coefficient of Expansion of Concrete and Reinforced Concrete at Below Normal Temperatures

Author(s): Carl Berwanger

Publication: Special Publication

Volume: 25

Issue:

Appears on pages(s): 191-234

Keywords: age; bridge decks; bridges (structures); composite construction (concrete & steel); concrete slabs; concretes; dynamic modulus of elasticity; low temperature; modulus of elasicity; reinforced concrete; reinforcing steels; research; strain gages; strains

Date: 1/1/1971

Abstract:
The dynamic modulus of the concrete and the coefficent of expansion of concrete and reinforced concrete slabs have been determined in the tests reported.