Title: Mass Concrete for Oroville Dam

Author(s): Lewis H. Tuthill, Robert F. Adams, and Donald R. Mitchell

Publication: Special Publication

Volume: 6

Issue:

Appears on pages(s): 179-198

Keywords:

Date: 1/1/1963

Abstract:
Reports the effect of various materials and various mix proportions on compressive strength at different ages, shrinkage, modulus of elasticity, and tensile splitting strength. Effect of curing conditions and the size of test cylinder are evaluated.