Title: Dynamic Shear Strength of Reinforced Concrete Beams

Author(s): R.H. Seabold

Publication: Symposium Paper

Volume: 42

Issue:

Appears on pages(s): 321-346

Keywords: beams (supports); bonding; building codes; computer programs; diagonal tension; dynamic loads; failure; modulus of elasticity; reinforced concrete; research; shear strength; shear tests; structural analysis; structural design; web reinforcement

Date: 1/1/1974

Abstract:
Theoretical and experimental work was done to study shear and diagonal tension in reinforced concrete beams for protective construction against the blast effects of nuclear and conventional weapons.




  