Title: Contribution of Aggregate Interlock and Dowel Forces to the Shear Resistance of Reinforced Beams with Web Reinforcement

Author(s): R.N. Swamy and A.D. Andriopoulos

Publication: Symposium Paper

Volume: 42

Issue:

Appears on pages(s): 129-168

Keywords: aggregate interlock; beams (supports); cracking dowels; failure; loads (forces); moment distribution; reinforced concrete; reinforcing steels; shear transfer; stress analysis; web reinforcement

DOI: 10.14359/17282

Date: 1/1/1974

Abstract:
Tests are reported to determine the contribution of aggregate interlock and dowel forces to the shear resistance of reinforced concrete beams with web reinforcement.




  