Friction Connection of Precast Concrete Construction

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Friction Connection of Precast Concrete Construction

Author(s): C.Y. Lin

Publication: Special Publication

Volume: 103

Issue:

Appears on pages(s): 27-46

Keywords: connections; friction; lead (metal); performance; plastics, polymers and resins; precast concrete; pressure; rubber; shear properties; strength; torsion; Construction

Date: 9/1/1987

Abstract:
This exploratory study was to investigate the feasibility of using friction-type connections in precast concrete construction. Tests were conducted to study the relationship between the friction capacity of precast concrete contact surfaces and general de