Title: Modified Compression-Field Theory for Reinforced Concrete Beams Subjected to Shear

Author(s): Vecchio, F. J., and Collins, M. P.

Publication: 318Reference

Volume: 19

Issue: 17

Appears on pages(s): pp. 219-223.

Keywords:

Date: 6/1/2008

Abstract:
ACI JOURNAL, Proceedings V. 83, No. 2, Mar.-Apr. 1986