Title: Estimating Prestress Losses

Author(s): Zia, P.; Preston, H. K.; Scott, N. L.; and Workman, E. B.

Publication: 318Reference

Volume: 18

Issue: 9

Appears on pages(s): pp. 32-38.

Keywords:

Date: 6/1/2008

Abstract:
Concrete International: Design & Construction, V. 1, No. 6, June 1979