Title: Tests to Determine the Lateral Distribution of Vertical Loads in a Long-Span Hollow-Core Floor Assembly

Author(s): Pfeifer, D. W., and Nelson, T. A.

Publication: 318Reference

Volume: 16

Issue: 15

Appears on pages(s): pp. 42-57.

Keywords:

Date: 6/1/2008

Abstract:
PCI Journal, V. 28, No. 6, Nov.-Dec. 1983