Title: Precast Concrete Wall Panels: Bowing, Warpage, and Movement

Author(s): Sheng Pao Sheng

Publication: Special Publication

Volume: 11

Issue:

Appears on pages(s): 57-63

Keywords:

Date: 1/1/1965

Abstract:
Investigations were made on several existing buildings, and the results analyzed. Some tentative conclusions as to bowing, warpage, and movement are presented here fur further discussion and study.