Title: Durability of Concrete With Multi-Component Binder

Author(s): W. Barry Butler

Publication: Symposium Paper

Volume: 104

Issue:

Appears on pages(s): 205-222

Keywords: abrasion resistance; admixtures; binders (materials); sorption; concrete durability; curing; fly ash; lignin and derivatives; reviews; water-cement ratio; water-reducing agents; Materials Research

DOI: 10.14359/1636

Date: 10/1/1987

Abstract:
During the past 50 years, there have been significant changes in the composition of general-purpose concrete. Along with changes in the performance of portland cement, changes have come about due to the inclusion of chemical and mineral admixtures,




  