Stands, Stadia, and Bowls

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Stands, Stadia, and Bowls

Author(s): Charles Wellford Leavitt

Publication: Journal Proceedings

Volume: 11

Issue: 8

Appears on pages(s): 576-584

Keywords: none

Date: 8/1/1915

Abstract:
The problem of handling crowds always has been most important in all stages of the development of civilization; it is one which has demanded the attention of many classes of thoughtful men.