Unit Costs in Construction

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Unit Costs in Construction

Author(s): Sanford E. Thompson

Publication: Journal Proceedings

Volume: 12

Issue: 2

Appears on pages(s): 347-350

Keywords: none

Date: 2/1/1916

Abstract:
The aim of this paper is to call attention to the necessity for more accurate estimates by architects, engineers and contractors, and to the possbility of reducing construction costs by a more thorough analysis and systematizing of the labor operations.