Title: Friction Tests of Concrete on Various Sub-Bases

Author(s): A.T. Goldbeck

Publication: Journal Proceedings

Volume: 13

Issue: 2

Appears on pages(s): 239-245

Keywords: none

Date: 2/1/1917

Abstract:
The rational design of any structure, whether it be a bridge or a pavement, necessitates a knowledge of the stresses to which it will be subjected.