Title: Treatment of Concrete Ornamental Elevated Stations, Dual System of Rapid Transit, New York City

Author(s): S.J. Vickers

Publication: Journal Proceedings

Volume: 13

Issue: 2

Appears on pages(s): 170-173

Keywords: none

Date: 2/1/1917

Abstract:
The City of New York, by the Public Service Commission of the First District, is now constructing what is known as the Dual System of Rapid Transit.