Title: Some Problems in Devising a New Finish for Concrete

Author(s): John J. Earley

Publication: Journal Proceedings

Volume: 14

Issue: 6

Appears on pages(s): 127-135

Keywords: none

Date: 6/1/1918

Abstract:
Reinforced concrete has long been jusified structurally but its appearance leaves much to be desired. In realization of its shortcomings in this respect, and in consideration of the importance of a work that would give to concrete an appearance commensurate with its structural value, an effort was made to acquire an intimate knowledge of what had been done towards this end.