Title: Recommended Practice for Portland Cement Stucco

Author(s): ACI Committee on Standard Recommended Practice for Portland Cement Stucco

Publication: Journal Proceedings

Volume: 15

Issue: 6

Appears on pages(s): 344-357

Keywords: none

Date: 6/1/1919

Abstract:
One of the fundamental considerations is successful stucco work is a suitable design of the structure for stucco.