Concrete Railway Track Support

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Concrete Railway Track Support

Author(s): A.C. Irwin

Publication: Journal Proceedings

Volume: 15

Issue: 6

Appears on pages(s): 153-172

Keywords: none

Date: 6/1/1919

Abstract:
Practically all expenditures that have been devoted to the improvement of railroad facilities and equipment may be traced to the necessity of obtaining greater traffic concentration.