In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
American Concrete Institute 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA
Phone: 1.248.848.3700 Fax: 1.248.848.3701 Staff Directory
Email Support
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: Fire Tests of Concrete Columns
Author(s): Walter A. Hull
Publication: Journal Proceedings
Volume: 15
Issue: 6
Appears on pages(s): 89-107
Keywords: none
Date: 6/1/1919
Abstract:A progress report of fire tests of concrete columns which are being conducted at the Pittsburgh laboratories of the Bureau of Standards was published in the Proceedings, of the American Concrete Instittute for 1918. The tests that have been made since that report was prepared extend the scope of the investigation by including additional aggregates and new applications of fire protective material. The tests reported in 1918 showed the behavior of columns of various types with coarse aggregates of Pittsburgh gravel and West Winfield, Pa. limestone. They also gave the results of two tests of columns which had had the protective concrete supplemented by the addition of other material, applied by plastering.