Report of Special Committee on Contractors Plant

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Report of Special Committee on Contractors Plant

Author(s): ACI Special Committee on Contractors Plant

Publication: Journal Proceedings

Volume: 17

Issue: 2

Appears on pages(s): 335-359

Keywords: none

Date: 2/1/1921

Abstract:
In line with decision reached in last year's Progress Report the Committee has confined its studies to plant used for handling concrete on building construction. The plant used for this particular type of work is in general basic for all concrete construction, subject to possible variation in the relation of the different untis to each other by reason of special conditions existing in different fields of construction.