Title: Test of a Flat-Slab Floor of the New Channon Building

Author(s): H.F. Gonnerman and F.E. Richart

Publication: Journal Proceedings

Volume: 17

Issue: 2

Appears on pages(s): 182-203

Keywords: none

Date: 2/1/1921

Abstract:
It is the object of this paper to present the results of a test made by the writers in July, 1920, upon a floor slab of the Henry Channon Building in Chicago.