Title: Concrete Pipe

Author(s): ACI Committee J-2

Publication: Journal Proceedings

Volume: 18

Issue: 2

Appears on pages(s): 318-321

Keywords: none

Date: 2/1/1922

Abstract:
Many of the railroads of the United States have for a number of years been using reinforced-concrete culvert pipe, a few manufacturing their own, others purchasing from outside pipe companies. Highway culvert pipe have also come into general use.