Title: Concrete Pipe, Drain Tile and Conduit
Author(s): ACI Committee P-7
Publication: Journal Proceedings
Volume: 21
Issue: 2
Appears on pages(s): 583
Keywords: none
Date: 2/1/1925
Abstract:
No meeting of the entire committee has been held since the 1924 convention of the Institute. However, three meetings of a sub-committee have been held for the purpose of revising the existing Tentative Standard Specifications for Reinforced-Concrete Sewer Pipe (P7C-24T), also to prepare other recommendations which are submitted below.