Title: Standard Specifications for Portland Cement Concrete Pavements: One-Course Portland Cement Concrete Street Pavement
Author(s): ACI Committee S-6
Publication: Journal Proceedings
Volume: 20
Issue: 2
Appears on pages(s): 716-723
Keywords: none
Date: 2/1/1924
Abstract:
It is the intent of these specifications cover the requirements for the materials and construction of Portland Cement Concrete Street Pavement wherein the concrete is of uniform proportion from top to bottom of slab.