Title: Contractor's Plant
Author(s): ACI Committee C-1
Publication: Journal Proceedings
Volume: 20
Issue: 2
Appears on pages(s): 648-656
Keywords: none
Date: 2/1/1924
Abstract:
The purpose of this paper is a general statement of the principles on which plant design depends and to give as thorough all exposition of these principles as is possible to present at this time, this without any restriction as to the type of project under consideration, but to illustrate particular types of concrete plants applicable to a certain set of given conditions. There is to be no discussion as to the relative merits of any type of equipment as applied to general uses, but rather to consider the use to which each particular device may be put so that it will work out to the best advantage.