Title: Weighing Concrete Aggregates on Highway Pavements

Author(s): R.W. Crum

Publication: Journal Proceedings

Volume: 20

Issue: 2

Appears on pages(s): 296-309

Keywords: none

Date: 2/1/1924

Abstract:
As a result of experience in weighing concrete aggregates upon two concrete paving contracts in 1923, the Iowa Highway Commission has adopted the actual weighing of aggregates on road pavement construction as standard practice.




  