Title: Tests of Colors for Portland Cement Mortars

Author(s): Raymond Wilson

Publication: Journal Proceedings

Volume: 23

Issue: 2

Appears on pages(s): 226-252

Keywords: none

Date: 2/1/1927

Abstract:
This is a progress report on an investigation of the effect of commercial pigments on the color, permanence of color and compressive strength of portland cement mortar.