Title: SP-190: High-Performance Fiber-Reinforced Concrete Thin Sheet Products

Author(s): Editors: Alva Peled, Surendra P. Shah, and Nemkumar Banthia

Publication: Special Publication

Volume: 190

Issue:

Appears on pages(s): 214

Keywords:

Date: 4/1/2000

Abstract:
SP190 The 11 papers in this Special Publication were presented at the ACI Spring Convention in Chicago, Illinois in March 1999, and represent worldwide advances in the development of high-performance fiber reinforced thin sheet products. The applications addressed include curtain walls, pipes, roof tiles, and repair/retrofit of existing structures. The manufacturing processes are discussed as well as the variety of natural and manufactured materials used.