Title: SP-189: High-Performance Concrete

Author(s): Editor: H.G. Russell

Publication: Special Publication

Volume: 189

Issue:

Appears on pages(s): 466

Keywords:

Date: 1/1/2000

Abstract:
A total of 25 papers are included in this Symposium Publication on HPC. The general topics include HPC bridges, HPC structural lightweight concrete, material science of HPC, and structural safety of HPC. Note: The individual papers are also available as .pdf downloads.. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP189