Title: SP-069: Applications of Polymer Concrete
Author(s): Editors: David W. Fowler and Lawrence E. Kukacka
Publication: Symposium Paper
Volume: 69
Issue:
Appears on pages(s): 228
Keywords:
Date: 8/1/1981
Abstract:
SP-69
A selection of topics covering basic development and applications of polymers in concrete. Contains 14 papers from a 1980 symposium on this subject. Research projects, special construction uses, industrial applications, performance studies, and types of polymer admixtures are reported.