Title: SP-034: Concrete for Nuclear Reactors
Author(s): Editor: Clyde E. Kesler
Publication: Symposium Paper
Volume: 34
Issue:
Appears on pages(s): 1766
Keywords:
Date: 1/1/1972
Abstract:
SP34
Contains a presentation from the International Symposium "Concrete for Nuclear Reactors," held in Berlin in 1970 plus additional selected papers and discussions, and a 365-entry annotated bibliography on concrete for radiation shielding. Subjects include: what the designer needs to know; concrete strength under different states of stress; behavior under long-term thermal influences; effects of neutron irradiation; and future research and development.