Title: SP-223: Investigating Concrete-Selected Works of Bryant and Katherine Mather
Author(s): Editors: Celik Ozyildirim and Shuaib Ahmad
Publication: Symposium Paper
Volume: 223
Issue:
Appears on pages(s): 259
Keywords:
Date: 10/1/2004
Abstract:
"In October 2000, the American Concrete Institute’s Technical Activities Committee approved publication of a commemorative compilation honoring Bryant Mather for his significant contributions to concrete technology. This publication, Investigating Concrete—Selected Works of Bryant and Katharine Mather, is the result of a cooperative effort by Mather, Celik Ozyildirim, and ACI Chief Engineer Shuaib Ahmad. It is divided into seven parts: potential of concrete; cementitious materials; aggregates; durability of concrete; petrographic examination of aggregates and concrete; specifications for use of concrete in transportation structures; and research and emerging technologies. This publication also includes an appendix with a bibliography of selected works of Bryant and Katharine Mather."
Note: The individual papers are also available as .pdf downloads.. Please click on the following link to view the papers available, or call 248.848.3800 to order.
SP223