Title: CP-26(89)A: Fundamentals of Proportioning Concrete Mixtures
Author(s):
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s):
Keywords:
Date: 4/1/1990
Abstract:
"VHS Tape"
Demonstrates basic procedures for proportioning normal weight concrete mixtures according to the absolute volume methods found in ACI publication 211.1 "Selecting Proportions for Normal, Heavyweight, and Mass Concrete."