Title: CP-16(04): Technician Workbook for ACI Certification of Concrete Laboratory Testing Technician Grade I
Author(s):
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s):
Keywords:
Date: 12/16/2003
Abstract:
Note: CP-16(04) is Out of Print. However, a newer version of this document exists. This document was replaced by CP-16(05).
This workbook orients the trainee/examinee to the Grade I certification program and provides the resources necessary to prepare for the required written and performance examinations. It also includes a suggested course outline, study questions, sample checklists, and a practice exam. Grade I certification covers ASTM standards: C 29, C 39, C 40, C 117, C 127, C 128, C 136, C 566, C 617, C 702, C 1231 and D 75.