Title: CP-14(85)A: Laboratory Testing -- Tape #3
Author(s): ACI Committee E902 and Portland Cement Association
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s):
Keywords:
Date: 4/1/1986
Abstract:
Three ASTM Standard Test Methods on aggregate are demonstrated. The ASTM tests covered are: C78-Flexural Strength of Concrete C123-Lightweight Pieces in Aggregate C192-Making and Curing Concrete Test Specimens in the Laboratory