Thin Plates Prestressed with Textile Reinforcement

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Thin Plates Prestressed with Textile Reinforcement

Author(s): H. W. Reinhardt, M. Kruger, and C. U. Grosse

Publication: Special Publication

Volume: 206

Issue:

Appears on pages(s): 355-372

Keywords: AR-glass, bending, carbon, concrete, prestressing, textile reinforcement

Date: 4/1/2002

Abstract:
Tests were carried out on thin plates either reinforced or prestressed with textiles. The textiles had a warp knitted structure with 10 mm mesh size. The two materials AR glass and carbon behaved completely different in the four-point bending experiments.. Pull-out tests with acoustic emissino measurements showed clearly that the different bond behaviour was the cause for such differences.