Title: Concrete of the Future

Author(s): Robert F. Blanks

Publication: Journal Proceedings

Volume: 45

Issue: 4

Appears on pages(s): 565-568

Keywords: no keywords

DOI: 10.14359/12170

Date: 4/1/1949

Abstract:
Mr. Blanks, in his remarks as retiring president, depicts what concrete miht be in 50 years in the future and discusses the role of the engineer in that era.