Title: Pumice - Lightweight Aggregate
Author(s): Leslie I. Neher
Publication: Journal Proceedings
Volume: 48
Issue: 9
Appears on pages(s): 65-75
Keywords: no keywords
Date: 9/1/1951
Abstract:
The growth of pumice production in the United States during recent years is worthy of note. Chemical and physical properties, mix design, presaturation of aggregates and the application of pumice aggregates in lightweight tilt-up and masonry construction are discussed.