Title: Free-Span Prestressed Concrete Bridge

Author(s): U. Finsterwalder

Publication: Journal Proceedings

Volume: 49

Issue: 11

Appears on pages(s): 225-232

Keywords: no keywords

Date: 11/1/1952

Abstract:
Short description of prestressing system and construction of the bridge over the Neckar river in Neckarrems, Germany, using a free-span prestressed concrete system.