Title: Corrugated Box Forms for Concrete Ribbed-Slab Construction

Author(s): H. C. Pfannkuche

Publication: Journal Proceedings

Volume: 50

Issue: 1

Appears on pages(s): 353-356

Keywords: no keywords

Date: 1/1/1954

Abstract:
Describes application of corrugated box form to pan construction and to slab-on-ground structures. Cost data are included.