Title: Waterstops in Articulated Concrete Construction
Author(s): E. A. Allen and E. C. Higginson
Publication: Journal Proceedings
Volume: 52
Issue: 9
Appears on pages(s): 83-91
Keywords: no keywords
Date: 9/1/1955
Abstract:
The problem of making watertight joints in thin-slab concrete structures is treated. Rubber waterstops commonly used by the Bureau of Reclamation are discussed and illustrated. Properties of the materials, fabrication and installation methods, and laboratory tests are described.