Abstract:
Authors have reviewed English literature on laboratory and field tests of creep of concrete. Rather than abstract each article, they present a general discussion of information regarding the creep behavior and the factors influenc-ing such behavior of plain and reinforced concrete. A list of 121 references is provided; 25 of these are specifically cited in the paper, but all have been considered in its preparation. This summary of published test, results is intended for the general reader and may serve as a starting point for those who wish to continue study of this subject.