Title: Research in Progress - 1978

Author(s): ACI Committee 115

Publication: Journal Proceedings

Volume: 75

Issue: 8

Appears on pages(s): 404-413

Keywords: cements;concrete construction;concretes;durablity;earthquake resistant structures;fire resistance;plain concrete;precast concrete;prestressed concrete;reinforced concrete;reinforcing materils;research;structural analysis;structural design.

Date: 8/1/1978

Abstract:
This compliation lists more than 200 research projects on concrete materials, structures, and construction currently in progress throughout the world. Each entry gives the project title, principal investigator(s), organization, and country.




  