Mitigation of Seismic Induced Diagonal Cracks in Concrete Columns by External Prestressing

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Mitigation of Seismic Induced Diagonal Cracks in Concrete Columns by External Prestressing

Author(s): M. Saatcioglu

Publication: Special Publication

Volume: 204

Issue:

Appears on pages(s): 195-216

Keywords: bridge columns; bridges; concrete columns; crack control; cracking; earthquake engineering; prestressed concrete; prestressing; retrofitting; seismic retrofit; shear design

Date: 8/1/2001

Abstract:
bridge columns; bridges; concrete columns; crack control; cracking; earthquake engineering; prestressed concrete; prestressing; retrofitting; seismic retrofit; shear design