Title: High Volume Fly Ash RCC for Dams: Freezing and Thawing Durability

Author(s): S. Jacobsen and 0. Lahus

Publication: Symposium Paper

Volume: 202

Issue:

Appears on pages(s): 315-330

Keywords: dilation; fly ash; freezing and thawing durability; RCC dam; saturation; service life; sustainable development

Date: 8/1/2001

Abstract:
dilation; fly ash; freezing and thawing durability; RCC dam; saturation; service life; sustainable development




  