Title: Use of Peat Ash in Concrete

Author(s): A. Heikkinen

Publication: Special Publication

Volume: 91

Issue:

Appears on pages(s): 449-462

Keywords: admixtures; ashes; compressive strength; concretes; peat.

Date: 2/1/1986

Abstract:
Peat ash is suitable for use as a constituent of concrete. The quality and quantity of admixtures and ash used in concrete have a strong influence on the development of compressive strength.