International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Showing 1-5 of 50 Abstracts search results

Document: 

SP369-04

Date: 

May 1, 2026

Author(s):

A. Dahal, Y. Wang, K. Wille

Publication:

Symposium Papers

Volume:

369

Abstract:

Ultra-High-Performance Concrete (UHPC) provides excellent mechanical properties and durability but often relies on high cement content, raising sustainability concerns. To enhance environmental performance, supplementary cementitious materials (SCMs), such as recycled glass powder (RGP), are increasingly used as partial cement replacements. The efficiency of RGP as a reactive SCM is strongly influenced by its dispersion behavior, which depends on the chemical composition of the cement pore solution, including its pH and ionic concentration. In this study, pore solutions were extracted using vacuum filtration and pressure squeezing at varying water-to-cementitious ratios (w/cm) and pressures. Results showed that higher w/cm increased calcium concentrations and decreased alkali and sulfur content, whereas pressure squeezing yielded solutions that closely resembled those in UHPC. Sedimentation tests were performed in RGP suspensions prepared in deionized (DI) water, untreated pore solution, and polycarboxylate ether (PCE) based high-range water-reducing admixture (HRWRA) treated pore solution. Results indicated that untreated pore solutions caused rapid agglomeration and settling of RGP, whereas PCE addition stabilized suspensions and improved dispersion. The study advances understanding of RGP dispersion behavior and supports the more efficient utilization of SCMs, enabling reduced cement demand and more sustainable UHPC production.

DOI:

10.14359/51750719


Document: 

CI4805Bermudez

Date: 

May 1, 2026

Author(s):

Manuel Bermudez, Chung-Chan Hung

Publication:

Concrete International

Volume:

48

Issue:

5

Abstract:

This paper re-evaluates existing definitions of tensile strain hardening in ultra-high-performance concrete (UHPC) materials and provides practical guidance for interpreting and reporting tensile stress–strain data, including identification of key parameters relevant to structural applications. This paper provides engineers with an overview of existing methods and recommends an approach that enables objective, consistent interpretation and reporting of the UHPC tensile stress–strain curve to qualify tensile strain-hardening properties for structural applications.

DOI:

10.14359/51750693


Document: 

CI4702El-Tawil

Date: 

February 1, 2025

Author(s):

Sherif El-Tawil, Musawer A. Saqif, William Hazelton, Jon Winckler, and Michael Clark

Publication:

Concrete International

Volume:

47

Issue:

2

Abstract:

Ultra-high-performance concrete (UHPC) is an advanced cementitious composite material with extraordinary mechanical and durability properties. This article discusses the construction of a short-span bridge using UHPC as well as the cost considerations associated with building an entire bridge with UHPC and reflects on lessons learned from the process.

DOI:

10.14359/51745608


Document: 

SP-363-6

Date: 

July 1, 2024

Author(s):

Kuo-Wei Wen, Manuel Bermudez, and Chung-Chan Hung

Publication:

Symposium Papers

Volume:

363

Abstract:

Ultra-high-performance concrete (UHPC) features tensile strain-hardening behavior and a high compressive strength. Existing studies on the shear behavior of UHPC structural members have been focused on prestressed UHPC girders. More experimental data of the shear behavior of non-prestressed UHPC beams are necessary to quantify the safety margin of shear designs for structures. Moreover, while the UHPC members in most studies did not contain coarse aggregate to strengthen their microstructure, the inclusion of coarse aggregate has been shown to substantially reduce the autogenous shrinkage and enhance the elastic modulus for UHPC materials, which is beneficial for structural applications of UHPC. This study experimentally investigated the shear failure behavior of eighteen non-prestressed rectangular UHPC beams. The experimental variables included the volume fraction of fibers, shear span-to-depth ratio of the beams, and coarse aggregate. The detailed shear failure responses of the UHPC beams were discussed in terms of the damage pattern, shear modulus, shear strength, shear strain, and strain energy. The test results showed that the inclusion of coarse aggregate increased the beam shear strength, and its enhancement became more significant with a higher volume fraction of fibers and a lower shear span-to-depth ratio of the beam. In addition to the experimental investigation, a shear strength model for non-prestressed rectangular UHPC beams that accounts for the interactive effect of the key design parameters was developed. An experimental database of the shear strength of the UHPC beams in existing studies was established to assess the performance of the proposed model. It was shown that the proposed model reasonably predicted the shear strength of the UHPC beams in the database with a higher accuracy and lower scatter compared to the results of existing models.

DOI:

10.14359/51742109


Document: 

SP-363-3

Date: 

July 1, 2024

Author(s):

Megan S. Voss, Daniel Alabi, Raid S. Alrashidi, Taylor A. Rawlinson, Christopher C. Ferraro, H. R. Hamilton, Joel B. Harley, and Kyle A. Riding

Publication:

Symposium Papers

Volume:

363

Abstract:

The movement of ultra-high-performance concrete (UHPC) toward wide scale acceptance within the concrete industry has generated interest in developing improved test methods to provide quality assurance for this material. Most test methods currently used to measure the tensile behavior of ultra-high-performance concrete require specialized testing equipment that is not typically owned by precast or ready-mix production facilities. These test methods provide reliable data for quality assurance of newly developed concrete mixes, but they are impractical as quality-control tests, which would need to be performed for every UHPC placement. This paper presents the development of a simple and inexpensive test to measure tensile strength and ductility for UHPC and serve as a quality-control test. This method was developed from the double-punch test, commonly referred to as the “Barcelona test,” but has been revised to incorporate substantial changes to the loading and data collection requirements to eliminate the need for expensive, specialized equipment. It was determined that the modified test method could produce reliable results using a load-controlled testing procedure with manually recorded data points taken every 0.635 mm (0.025 inches) of vertical displacement for ductile concrete specimens. It was also determined that specimen surface grinding, loading rate, and punch alignment did not significantly influence the test results. However, the fabrication of the specimens, specifically the rate and method at which the molds were filled, had a significant effect on the results. Accordingly, any recommended standardized test method based off of this procedure should have requirements on specimen fabrication.

DOI:

10.14359/51742106


12345...>>

Results Per Page