ACI Global Home Middle East Region Portal Western Europe Region Portal
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Topics In Concrete
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Showing 1-5 of 136 Abstracts search results
Document:
24-248
Date:
January 19, 2026
Author(s):
Fen Zhou, Lijuan Li, Yunxing Du, Fei Peng, Deju Zhu
Publication:
Structural Journal
Abstract:
To promote the application of fiber-reinforced polymer (FRP) bars reinforced ultra-high-performance seawater sea-sand concrete (FRP-UHPSSC) structures in marine construction, four-point static bending tests were carried out on 16 FRP-UHPSSC beams with different reinforcement ratios, height of cross-section, and type of FRP bars to investigate the ultimate load-carrying capacity, the midspan deflection, and the failure modes of the beams. The experimental results show that all the test beams are brittle failures, and the failure mode of the beams is shear failure when the ratio of the actual reinforcement ratio to the balanced one is higher than 2.73. Increasing the reinforcement ratio and the beam section height both improve the bending moment at ultimate load and the flexural stiffness at the service limit state. The Steel-FRP composite bars (SFCB) reinforced UHPSSC beams have the maximal bending moment at ultimate load, and the basalt fiber reinforced polymer (BFRP) bar reinforced UHPSSC beams have the optimal ductility. The deviation of ultimate bending moment and midspan deflection obtained by the proposed calculation method is reduced from 7.5 to 2.8%, and from 15 to 3%, respectively, compared with current specifications for FRP-reinforced concrete structures.
DOI:
10.14359/51749490
25-079
January 12, 2026
Weibo Tan, Peiyuan Chen, Ying Xu, Chunning Pei, Yi Fang, Jin Li, Xin Qian, and Jialai Wang
Materials Journal
To address the autogenous shrinkage issue of ultra-high-performance concrete (UHPC), internal curing technology has shown great potential in resolving this challenge by providing additional moisture. To further improve its curing efficiency, this study proposes an innovative internal curing technology that can significantly reduce autogenous shrinkage without increasing the amount of internal curing water or compromising mechanical strength. This approach utilizes perforated cenospheres (PCs) as internal curing agents while substituting internal curing water with urea solutions. In addition to replenishing water, urea solutions, once released into the cement paste, can react with portlandite. This reaction generates CaCO₃; owing to the intrinsic properties of CaCO₃, it has a larger macroscopic volume and a much higher elastic modulus than portlandite. This approach effectively reduces chemical shrinkage while concurrently increasing the stiffness of the cement paste, thereby achieving a significant reduction in autogenous shrinkage. As a result, replacing water with 3% urea solution in PCs enhances the autogenous shrinkage of UHPC, reducing it from less than 50% to over 90%.
10.14359/51749446
25-265
December 18, 2025
Fayez Moutassem
This study presents a machine learning–driven framework for the sustainable design of ultra-high-performance concrete (UHPC) mixtures with a focus on maximizing flexural strength while minimizing material cost and embodied CO₂ emissions. A curated dataset of 333 UHPC mixtures was developed, incorporating 13 input features including binder composition, steel fiber dosage, and curing parameters. A Bayesian Neural Network (BNN) was trained to predict flexural strength with high accuracy (R² = 0.936, RMSE = 1.37 MPa, MAE = 1.09 MPa), supported by residual analysis confirming minimal prediction bias and robust generalization. SHAP analysis was used to interpret model predictions and identify key drivers of flexural behavior—namely, curing time, steel fiber dosage, and silica fume content. The BNN was coupled with the NSGA-III algorithm to perform multi-objective optimization and generate Pareto-optimal UHPC mixtures. A utility-based scoring method was introduced to select designs aligned with different project priorities—enabling the identification of fiber-rich, high-strength mixtures as well as low-emission, cost-efficient alternatives. The framework supports field-level implementation and is well-suited for integration with sustainability rating systems such as LEED or Envision. It provides a transparent, generalizable, and industry-ready tool for intelligent UHPC mixture optimization, advancing data-driven design practices for green infrastructure applications.
10.14359/51749415
25-134
December 11, 2025
Sahil Bansal
Advances in concrete material science have led to the development of a new class of cementitious materials, namely ultra-high-performance concrete (UHPC), which offers superior mechanical and durability properties. The control and characterization of the fresh properties of UHPC are crucial for successful mixture design. Among the methods for evaluating these properties, the mini-cone test has gained prominence due to its practicality. It requires smaller sample volumes than the standard slump cone test, making it especially suited for laboratory assessments of UHPC mixtures. In contrast, the slump flow test is the simplest and most widely used test for both laboratory and field testing of concrete. This study aims to establish a correlation between mini-cone flow and standard slump flow test results. A linear relationship is identified, which forms the basis for proposing consistency classes for UHPC using mini-cone flow values. These proposed classes align with the established consistency classifications for self-compacting concrete.
10.14359/51749383
24-476
December 8, 2025
Giwan Noh, Seung Heon Lee, and Thomas H.-K. Kang
Ultra-high performance concrete (UHPC) is a forward-looking material ideal for use in large-scale civil infrastructure systems. However, due to its unique mix, when UHPC is used in actual structures in conjunction with materials like steel reinforcement, it may lead to unexpected behavior. Therefore, this study analyzed the behavior of reinforced UHPC (R-UHPC) for use in actual structures, focusing specifically on beams among various structural components, with a particular emphasis on their flexural behavior. For this purpose, the study collected and comprehensively analyzed experimental data from flexural tests of R-UHPC beams conducted to date, identifying basic mechanics, peculiarities, and considerations in structural design. This study highlights that, besides the commonly known longitudinal reinforcement ratio, numerous factors such as beam length, height, number of tension reinforcement layers, strength, etc., can influence the flexural behavior of R-UHPC beams and demonstrate how these elements impact the performance.
10.14359/51749375