ACI Global Home Middle East Region Portal Western Europe Region Portal
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Topics In Concrete
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Showing 1-1 of 1 Abstracts search results
Document:
CI4501Chopperla
Date:
January 1, 2023
Author(s):
Krishna Siva Teja Chopperla, Sivakumar Ramanathan, Robert J. Moon, O. Burkan Isgor, and W. Jason Weiss
Publication:
Concrete International
Volume:
45
Issue:
1
Abstract:
The addition of cellulose nanomaterials to cementitious materials has been shown to alter rheology, setting times, degree of hydration, and mechanical properties The article discusses implementation of cellulose nanocrystals (CNCs) in three full-scale concrete placements (parking lot, bridge girder, and slab-on-ground) to examine the potential of using CNCs in the field.
DOI:
10.14359/51738464