International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Showing 1-5 of 106 Abstracts search results

Document: 

CI4710Heitmeyer

Date: 

October 1, 2025

Author(s):

Keila Heitmeyer

Publication:

Concrete International

Volume:

47

Issue:

10

Abstract:

Cold weather conditions pose constructability challenges when placing and testing to ensure a sound product. The key to successfully executing field work in cold weather conditions is to plan diligently while considering recommendations from ACI 306R-16, “Guide to Cold Weather Concreting.”

DOI:

10.14359/51749210


Document: 

CI4601Klinger

Date: 

January 1, 2024

Author(s):

James Klinger, Joseph F. Neuber Jr., Jeffrey Ondo, and Bruce A. Suprenant

Publication:

Concrete International

Volume:

46

Issue:

1

Abstract:

Placing and finishing of concrete slabs with portland-limestone cement (Type IL cement) may create issues for some contractors, and bleeding rate is a major factor. The article discusses saw cutting, cold weather protection, post-tensioning, and form removal, as well as best practices and strategies to minimize risks during floor slab finishing and early-age, strength-critical construction with Type IL cement.

DOI:

10.14359/51740317


Document: 

CI4601Q&A

Date: 

January 1, 2024

Publication:

Concrete International

Volume:

46

Issue:

1

Abstract:

Two documents from ACI Committee 306, Cold Weather Concreting, include different definitions for cold weather. This Q&A discusses both definitions and explains which definition should be incorporated into project specifications and project submittals.

DOI:

10.14359/51740326


Document: 

SP-354_22

Date: 

July 1, 2022

Author(s):

Mario Collepardi, Jean Jacob Ogoumah Olagot and Roberto Troli

Publication:

Symposium Papers

Volume:

354

Abstract:

The present paper preliminarily illustrates the mechanism of damages caused by the alkali-silica reaction (ASR) between the high alkali content of the dry shake-hardener due to the high cement content on the top of the concrete industrial floors and the alkali-reactive coarse aggregate in the concrete substrate. To mitigate or prevent these damages a special dry shake-hardener, based on the partial replacement of the Portland cement by siliceous fly ash, is used. The beneficial influence of the fly ash, as well as that of other fine pozzolanic materials, is due to the distribution of a very large number of amorphous silica-based fine particles which can potentially react with the alkali in the same way as the amorphous or badly crystallized silica of the alkali-reactive coarse aggregates. The introduction of a very high number of pozzolanic particles significantly reduces the alkali availability for the reaction with the few alkali-reactive coarse aggregates. In other words, the alkalis instead of concentrating their aggression on a few grains of the alkali-reactive coarse aggregates, usually 5 to 15 mm (2 to 6 in.) in size, spread their action on a large number of very fine pozzolanic particles so that their expansive and destructive power is lost. However, another problem can arise when the Portland cement is partially replaced by fly ash due to the longer setting time, particularly in cold weather, of the dry shake-hardener, so that the workers must wait a very long time before the mechanical troweling and the opening of the finished surface to the pedestrian traffic. To avoid this drawback a combined use of the siliceous fly ash and a setting accelerator, based on tetra-hydrate calcium nitrate in powder form [4H2O∙Ca(NO3)2 > 4H2O∙CaO∙N2O5 > H4CN2] has been studied at three different temperatures: 35°C (95°F), 20°C (68°F) and 5°C (41°F). In warm weather, at temperatures as high as 35°C (95°F), there is no need for H4CN2 since the Portland cement hydration occurs at a very great rate and only the dry shake-hardener containing fly ash without H4CN2 can be applied within few hours and incorporated into the concrete substrate. At 20°C (68°F) the delay in the setting times caused by the partial replacement of Portland cement by fly ash can be compensated by the use of H4CN2 at 1% by weight of the cementitious materials. In cold weather, such as that caused by a temperature as low as 5°C (41°F), a much higher percentage of H4CN2, up to 5% by weight of the cementitious materials, must be used to reduce the setting times at approximately the same values as those recorded at 20°C (68°F) when the dry shake-hardener without fly ash is used.

DOI:

10.14359/51736078


Document: 

CI4212Q&A

Date: 

December 1, 2020

Publication:

Concrete International

Volume:

42

Issue:

12

Abstract:

Q: Last winter, we placed concrete grade beams for an industrial building. A technician from the owner’s testing agency took test cylinders but left them unprotected in the cold weather for a week. At 28 days, the average cylinder compressive strength was 2750 psi. Because this was far below the specified fc of 6000 psi, the engineer required three cores to be taken to evaluate the in-place concrete strength. The individual core compressive strengths were 4940, 4970, and 5370 psi, resulting in an average strength of 5090 psi (84.8% of fc). The engineer rejected the concrete on the basis that the ACI 318-19 Code1 requires the average core strength to equal 85% of the specified strength. In this case, 0.85 fc = 5100 psi, so isn’t the average core strength of 5090 psi close enough?

DOI:

10.14359/51730384